{"product_id":"ieej-20250304x01101-003","title":"原子力発電所撤去EPDMケーブルの電気絶縁特性 ―加速劣化手法の保守性―","description":"\u003cp\u003e\u003cstrong\u003eカテゴリ: \u003c\/strong\u003e研究会(論文単位)\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e論文No: \u003c\/strong\u003eDEI25069,EWC25007\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eグループ名: \u003c\/strong\u003e【A】基礎・材料・共通部門 誘電・絶縁材料\/【B】電力・エネルギー部門 電線・ケ－ブル合同研究会\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e発行日: \u003c\/strong\u003e2025\/03\/04\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eタイトル(英語): \u003c\/strong\u003eElectrical Insulation Properties of an EPDM Cable Removed from a Nuclear Power Plant - Conservativeness of the Accelerated Aging Method -\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e著者名: \u003c\/strong\u003e大木  義路(早稲田大学),平井  直志(早稲田大学),田中 康寛(東京都市大学)\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e著者名(英語): \u003c\/strong\u003eYoshimichi  Ohki(Waseda University),Naoshi Hirai(Waseda University),Yasuhiro Tanaka(Tokyo City University)\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eキーワード: \u003c\/strong\u003e電気ケーブル|電流積分法|高分子絶縁|経年劣化|保守性|Electric cable|current integration method|polymeric insulation|aging|conservativeness\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e要約(日本語): \u003c\/strong\u003e沸騰水型軽水炉の格納容器内において長時間使用されたのちに撤去されたケーブルRと同種の新品ケーブルに，撤去ケーブルが受けたであろう経年変化を「時間依存データの重ね合わせ」に基づく加速模擬手法により模擬的に与えた。その上で，両ケーブルに，SAとLOCAと呼ばれる二つの事故時に想定される放射線照射と水蒸気曝露を与え，その後直流電圧印加によりケーブル絶縁体に流れる漏れ電流を電流積分法により測定した。その結果，ケーブルRと模擬的に経年変化を与えられたケーブルAD間で，ほぼ同一の絶縁特性，あるいは，ケーブルADの方が\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e要約(英語): \u003c\/strong\u003eA new cable of the same type as cable R, which was removed after being used for a long time in the containment vessel of a boiling water nuclear power reactor, was subjected to accelerated aging based on \"superposition of time-dependent data'' to simulate the aging deterioration that cable R would have experienced. Then, both cables were exposed to radiation and water steam, which would be expected during two types of accidents, SA and LOCA. After that, a DC voltage was applied, and the current integration method was applied to measure the leakage current passing through each cable insulation. As a result, in most cases, cable R and cable AD subjected to simulated aging exhibit almost the same insulation properties, or cable AD exhibits slightly worse insulation properties than cable R. This confirms that the accelerated simulation method has conservativeness.\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e本誌: \u003c\/strong\u003e\u003ca href=\"\/products\/ieej-20250304x01101\"\u003e2025年3月7日誘電・絶縁材料\/電線・ケ－ブル合同研究会\u003c\/a\u003e\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e本誌掲載ページ: \u003c\/strong\u003e17-24 p\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003e原稿種別: \u003c\/strong\u003e日本語\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003ePDFファイルサイズ: \u003c\/strong\u003e1,597 Kバイト\u003c\/p\u003e","brand":"IEEJ-P10","offers":[{"title":"冊子印刷（一般価格660円\/会員価格440円） \/ A4 \/ 8","offer_id":46408150745327,"sku":"IEEJ-20250304X01101-003-PRT","price":660.0,"currency_code":"JPY","in_stock":true},{"title":"PDFダウンロード（一般価格330円\/会員価格220円） \/ A4 \/ 8","offer_id":46408609792239,"sku":"IEEJ-20250304X01101-003-PDF","price":330.0,"currency_code":"JPY","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0718\/9512\/2159\/files\/IEEJ-KENKYUKAI_086384fd-c396-4f4e-a111-16f9764437f5.png?v=1745233376","url":"https:\/\/ieej.bookpark.ne.jp\/products\/ieej-20250304x01101-003","provider":"電気学会 電子図書館","version":"1.0","type":"link"}